(Solved): 9. Construct a 3D surface plot using Matlab (or any other plotting program) of Rockwell \( \mathrm ...



9. Construct a 3D surface plot using Matlab (or any other plotting program) of Rockwell \( \mathrm{F} \) hardness after annea10. Does annealing have a greater effect on relative change in hardness in the specimen with \( 40 \% \) CW target or \( 5 \%

9. Construct a 3D surface plot using Matlab (or any other plotting program) of Rockwell \( \mathrm{F} \) hardness after annealing (z-axis) \( v s \). actual \( \% \mathrm{CW} v s \). Annealing Temperature (8 temperatures) (in \( \mathrm{x} \) - and \( \mathrm{y} \)-axes). You are not required to include \( 0 \% \mathrm{CW} \), because we did not anneal any bars with \( 0 \% \mathrm{CW} \). The data before annealing should be plotted at \( 200^{\circ} \mathrm{C} \). You are not required to include error bars. Including axis labels with units. Include a figure number, title, and descriptive caption. (15 pts) 10. Does annealing have a greater effect on relative change in hardness in the specimen with \( 40 \% \) CW target or \( 5 \% \) CW target? Why? (Describe both the driving force and the physical mechanism for the change in hardness with annealing). (10 pts)


We have an Answer from Expert

View Expert Answer

Expert Answer


Ans 10 . The driving force for recrystalization comes from the energy stored in the cold worked areas of the copper. The physical mechanism